Titolo | The influence of high-temperature sintering on microstructure and mechanical properties of free-standing APS CeO2-Y2O 3-ZrO2 coatings |
---|---|
Tipo di pubblicazione | Articolo su Rivista peer-reviewed |
Anno di Pubblicazione | 2010 |
Autori | Alfano, M., Di Girolamo G., Pagnotta L., Sun D., Zekonyte J., and Wood R.J.K. |
Rivista | Journal of Materials Science |
Volume | 45 |
Paginazione | 2662-2669 |
ISSN | 00222461 |
Parole chiave | Air plasma spray, Annealing time, Before and after, Cerium compounds, Coating microstructures, Depth-sensing nanoindentation, Elastic moduli, Elasticity, hardness, High-temperature sintering, Image analysis, Isothermally annealed, Mechanical properties, Microstructural modification, Microstructure, Microstructure and mechanical properties, Nanoindentation, NO phase, Phase shifters, Phase stability, Plasma spraying, Protective coatings, Scanning electron microscopy, Sintering, Stabilized zirconia, Thermal aging, Vickers microindentation, X ray diffraction, X ray diffraction analysis, Young's Modulus, Yttria stabilized zirconia, Zirconia |
Abstract | In this study, ceria-yttria co-stabilized zirconia (CYSZ) free-standing coatings, deposited by air plasma spraying (APS), were isothermally annealed at 1315 °C in order to explore the effect of sintering on the microstructure and the mechanical properties (i.e., hardness and Young's modulus). To this aim, coating microstructure, before and after heat treatment, was analyzed using scanning electron microscopy, and image analysis was carried out in order to estimate porosity fraction. Moreover, Vickers microindentation and depth-sensing nanoindentation tests were performed in order to study the evolution of hardness and Young's modulus as a function of annealing time. The results showed that thermal aging of CYSZ coatings leads to noticeable microstructural modifications. Indeed, the healing of finer pores, interlamellar, and intralamellar microcracks was observed. In particular, the porosity fraction decreased from 10 to 5% after 50 h at 1315 °C. However, the X-ray diffraction analyses revealed that high phase stability was achieved, as no phase decomposition occurred after thermal aging. In turn, both the hardness and Young's modulus increased, in particular, the increase in stiffness (with respect to "as produced" samples) was equal to 25%, whereas the hardness increased to up to 60%. © 2010 Springer Science+Business Media, LLC. |